The outer surface of a steel alloy is to be hardened by increasing its carbon content. The carbon is to be supplied from an external carbon-rich atmosphere, which is maintained at an elevated temperature. A diffusion heat treatment at 825°C for 12 min increases the carbon concentration to 0.70 wt% at a position 1.6 mm below the surface. Estimate the diffusion time required at 640°C to achieve this same concentration also at a 1.6 mm position. Assume that the surface carbon content is the same for both heat treatments, which is maintained constant. The preexponential and activation energy values for the diffusion of carbon in the iron are 8.5 × 10-6 m2/s and 82.2 kJ/mol, respectively.

ansver
Answers: 2

Another question on Engineering

question
Engineering, 04.07.2019 18:10
Ajournal bearing has a journal diameter of 3.250 in with a unilateral tolerance of 20.003 in. the bushing bore has a diameter of 3.256 in and a unilateral tolerance of 0.004 in. the bushing is 2.8 in long and supports a 700-lbf load. the journal speed is 900 rev/min. find the minimum oil film thickness and the maximum film pressure for both sae 20 and sae 20w-30 lubricants, for the tightest assembly if the operating film temperature is 160°f. a computer code is appropriate for solving this problem.
Answers: 3
question
Engineering, 04.07.2019 18:20
Inadequate stores control is not an obstacle to effective work order system. (clo4) a)-true b)-false
Answers: 3
question
Engineering, 04.07.2019 18:20
Describe one experiment in which the glass transition temperature and melting temperature of a totally amorphous thermoplastic material can be determined. show the relevant experimental results in a diagram which should be properly annotated with the two temperatures clearly marked. what is likely to happen to the curve in the diagram if the amorphous polymer is replaced by a thermosetting type?
Answers: 2
question
Engineering, 04.07.2019 19:10
Estimate the change in specific internal energy au and specific enthalpy h from inlet to outlet for ethylene glycol (a liquid) flowing through each of the following devices: (a) a heat exchanger where the glycol temperature increases from 20 °c to 80 °c; (b) a pump operating at about 25 °c and increasing the glycol pressure from 100 kpa to 8 mpa.
Answers: 2
You know the right answer?
The outer surface of a steel alloy is to be hardened by increasing its carbon content. The carbon is...
Questions
question
Mathematics, 02.03.2020 22:55
question
History, 02.03.2020 22:55
question
Mathematics, 02.03.2020 22:55